Mechanical Properties Metric English Comments
Izod Impact, Notched 3.09 J/cm
5.79 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Izod Impact, Notched 3.09 J/cm
5.79 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Izod Impact, Notched 3.09 J/cm

@Thickness 3.20 mm
5.79 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2312 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 3.09 J/cm

@Thickness 3.20 mm
5.79 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 3.09 J/cm
5.79 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Izod Impact, Notched 3.09 J/cm
5.79 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Izod Impact, Notched 3.09 J/cm

@Temperature 23.0 °C
5.79 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl ENV85 PPE+PS (Asia Pacific)
Low heat, flame retardant, extrusion grade PPO/HIPS alloy.Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 3.09 J/cm

@Temperature 23.0 °C
5.79 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 3.09 J/cm
5.79 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific)
LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Copyright © lookpolymers.com All Rights Reserved