Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.0678 - 2.1356 J/cm @Temperature -40.0 - -20.0 °C |
2.0004 - 4.0009 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 1.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 1.0678 - 2.1356 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 4.0009 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.05 J/cm Grade Count:9 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.05 J/cm Grade Count:9 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.850 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.850 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Temperature -40.0 - -40.0 °C |
2.0004 - 2.0004 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.07 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 1.0678 - 1.0678 J/cm @Thickness 3.17 - 3.17 mm |
2.0004 - 2.0004 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 1.07 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched | 1.0678 J/cm | 2.0004 ft-lb/in | ASTM D256 |
Stratasys® ABS ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur.. |