Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
M. Holland Company PS20 Polystyrene, Ignition Resistant
(discontinued **) Additives: Ignition ResistantFeatures: Flame RetardantUses: Appliance Components, Business Equipment, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1520Processing Method: Injection Mol.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PBT GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: Natural ColorTPCI# 8649111Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Izod Impact, Notched | 1.07 J/cm @Thickness 3.17 mm |
2.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%) and Heat StabilizerFeatures: Lubricated, Good Wear Resistance, Heat Sta.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN2L PPE+PS (Asia Pacific) PPE+PS GF20%, hydrolytic stability |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ISO 180/A |
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature 22.8 °C |
2.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PA123G25 Nylon 66, 25% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylon® NSG-440A-H 60% Ceramic and Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.07 J/cm @Temperature -40.0 °C |
2.00 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Izod Impact, Notched | 1.07 - 4.27 J/cm | 2.00 - 8.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Izod Impact, Notched | 1.07 - 4.81 J/cm | 2.00 - 9.00 ft-lb/in | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® GFN 6633 Glass Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
M. Holland Company IS330 Polystyrene, High Impact
(discontinued **) Features: Impact ModifiedUses: Audio Tapes, Household Goods, ToysApprovals: FDA 21 CFR 177.1640Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Izod Impact, Notched | 1.07 J/cm | 2.00 ft-lb/in | ASTM D256 |
Ecomass® 5100TU96 Tungsten Filled SEBS Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled SEBS Base ResinVery FlexibleInformation provided by Technical.. |