Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 153 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 153R PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. Internal mold release. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hylex® P1017L Polycarbonate, Unreinforced, High Flow, Mold Release Information provided by Ravago. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate Information provided by Ravago |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific) Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Global PC-1408 General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Global PC-FR2 UL Recognized 94V-2 Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade Medium FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR IM BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: BlackTPCI# 9993101Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 15 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content Features: Good flowHigh rigidityGood toughnessHigh strengthLow viscosityGood mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 7.48 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 0614UV UV Stabilized Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 22.8 °C |
14.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 7.48 J/cm @Temperature -50.0 °C |
14.0 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Dow Prevail® 3100 ABS + Polyurethane PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used .. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Adell YS-10 PC Alloy |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Applied Composites 179 Polyester SMC Industry Application: TransportationProduct Application: Auto InteriorsInformation provided by Applied Composites Corporation. |
|||
Izod Impact, Notched | 7.48 J/cm | 14.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 827B Nylon 6 High impact, black, economy grade. Also available as: 827SB - Heat Stabilized, Black and 827SH - Heat Stabilized & UV Stabilized for Weatherability, Black.Data provided by the manufacturer |