Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.45 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Izod Impact, Notched | 6.48 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2289 PC Lexan* LUX2289 resin is an injection molding grade with high light reflectance |
|||
Izod Impact, Notched | 6.48 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Izod Impact, Notched | 6.47 J/cm @Temperature -30.0 °C |
12.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.47 J/cm @Temperature -30.0 °C |
12.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.47 J/cm @Temperature -30.0 °C |
12.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.47 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
Izod Impact, Notched | 6.47 J/cm @Temperature 23.0 °C |
12.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX6601 PPE+PA66 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.47 J/cm | 12.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX6601 PPE+PA66 (Asia Pacific) |
|||
Izod Impact, Notched | 6.46 J/cm | 12.1 ft-lb/in | LAB034 |
ExxonMobil Mytex™ AS33L-07VS rubber modified polypropylene with good impact and flow properties for automotive exterior applications.Information provided by ExxonMobil Chemical |
|||
Izod Impact, Notched | 6.48 J/cm @Thickness 3.17 mm |
12.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC-1212FRO Natural, Flame Retardant Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |