Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.892 J/cm @Thickness 3.20 mm |
1.67 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 425 General Purpose HIPS Key features: High-impact General Use. Common Uses: Office appliances, home appliances, various kitchenware, general merchandise, toys, leisure goods, etc.HIPS is a functional resin made by copolym.. |
|||
Izod Impact, Notched | 0.892 J/cm @Thickness 3.20 mm |
1.67 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HI 450PG High Gloss HIPS Common Uses: Monitor swivels, washers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance.Data pr.. |
|||
Izod Impact, Notched | 0.892 J/cm @Thickness 3.20 mm |
1.67 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo MIB 237 Blow Molding HIPS Key features: Good-profiling, Thin-layer Molding. Common Uses: It is used exclusively as a container for fermented milk beverages.HIPS is a functional resin made by copolymerization of styrene monom.. |
|||
Izod Impact, Notched | 0.892 J/cm @Thickness 3.20 mm |
1.67 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo MIB IT Blow Molding HIPS Key features: Vacuum Molding. Common Uses: Stirred type yot container.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resis.. |
|||
Izod Impact, Notched | 0.890 J/cm | 1.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics REMEX VR4831 PBT 15% Glass filled PBT, Flame retardant, UL Recognized, Utility grade, Black color only |
|||
Izod Impact, Notched | 0.890 J/cm | 1.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Izod Impact, Notched | 0.890 J/cm @Temperature 23.0 °C |
1.67 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.890 J/cm | 1.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Izod Impact, Notched | 0.890 J/cm @Temperature -30.0 °C |
1.67 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts.. |
|||
Izod Impact, Notched | 0.890 J/cm @Temperature -30.0 °C |
1.67 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
Izod Impact, Notched | 0.890 J/cm | 1.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
Izod Impact, Notched | 0.890 J/cm | 1.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |