Mechanical Properties Metric English Comments
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E-854-10/390-B-ERYB White PVC Compound
Heavy metal free PVC compound recommended for extrusion of profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 836-10/185-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 854-10/150-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 854-10/185-ERYB White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 855-10/150-ERYB-PO White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.448 J/cm

@Temperature 22.8 °C
0.840 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Sinpolene GPP1615/2 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 15% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; ..
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
PlastxWorld Veroplas PB2001F Nylon 66
flame retarded (UL94 V0), unfilled injection molding gradeInformation provided by PlastxWorld Inc.
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
PlastxWorld Veroplas PB5300 Nylon 66
general purpose, 30% mineral filled injection molding gradeInformation provided by PlastxWorld Inc.
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accuguard Polypropylene HP0369V2CSL Homopolymer Flame Retardant Copper Stabilized
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334M40CL Mica Reinforced Coupled
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336C20L Calcium Reinforced
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336C30L Calcium Reinforced
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336M10L Mica Reinforced
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339G20CL Glass Reinforced Coupled
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 841-08/184-A-ERYB Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.448 J/cm
0.840 ft-lb/in
ASTM D256
Aclo Accutech SAN SAN930G30L Glass Reinforced
Izod Impact, Notched >= 0.448 J/cm
>= 0.840 ft-lb/in
Method A; ASTM D 256
Karina E 841-08/184-Y-ERYB Beige PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.