Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 J/cm @Thickness 6.35 mm |
0.400 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 51 KC General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 30-2000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers SAN 279 Water White Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers SAN 290 High Flow Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers SAN 300 Natural Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | 73°F; ASTM D256 |
M. Holland Company GS230WC Polystyrene, Specialty High clarityCrystallineHigh heat resistanceGood mold releaseApplications: BottlesLabwareVials |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
I. Stern N2380 High Heat Crystal Polystyrene Features:High Molecular WeightExcellent Optical PropertiesApplicationsOPSFoamed TraysThick Walled Injection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. St.. |
|||
Izod Impact, Notched | 0.214 - 0.374 J/cm | 0.400 - 0.700 ft-lb/in | ASTM D256 |
Ineos H36G-00 Polypropylene Homopolymer This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 .. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D 638 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature -30.0 °C |
0.400 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 4181T Injection Molding Polypropylene Homopolymer with Antistat, ESCR AdditivesApplications: For general purpose injection molding applications such as closures.Formolene 4181T is a low viscosity, highly isotactic polypropylene homopoly.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature -30.0 °C |
0.400 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
A. Schulman POLYFORT™ FPP 1842 Homopolymer Polypropylene DescriptionPolyfort® FPP 1842 is a high stiffness, high heat resistant filled homopolymer polypropylene developed especially for instrument panel clusters. It is opaque to high intensity light.Inf.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 4100T Injection Molding Polypropylene Homopolymer with ESCR AdditivesApplications: Closures, small appliances, housewares and toys.Formolene 4100T is a low viscosity, highly isotactic polypropylene homopolymer designed for various injec.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256A |
Braskem CP360H Homopolymer Polypropylene Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256A |
Braskem F350HC2 High Crystallinity Homopolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256A |
Braskem ZS-751 Homopolymer Polypropylene Description: Superior stiffness, good static charge dissipation, excellent mold release, nucleated.Applications: Suggested uses include closures, overcaps, cosmetic packaging, disposable cutlery.Pro.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics EA3130 High Heat Crystal Polystyrene Product CharacteristicsAdditive FreeFood Contact CompliantTypical ApplicationsMedical PartsColor Concentrate CarrierLow Profile AdditivesInformation provided by AmericasStyrenics LLC. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 |
Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
Izod Impact, Notched | 0.214 J/cm | 0.400 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Quadrant PVC Polyvinyl Chloride, Type I, Grade 1 (ASTM Product Data Sheet) |