Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.0500 J/cm - NB | 0.0937 ft-lb/in - NB | Average value: 1.04 J/cm Grade Count:174 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.0500 - 7.50 J/cm @Temperature -40.0 - 0.000 °C |
0.0937 - 14.1 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 2.43 J/cm Grade Count:55 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.0500 J/cm | 0.0937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.0500 J/cm | 0.0937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.0500 J/cm | 0.0937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.0500 J/cm | 0.0937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.0500 J/cm | 0.0937 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature -30.0 °C |
0.0937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature -30.0 °C |
0.0937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature -30.0 °C |
0.0937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 0.000 °C |
0.0937 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.0500 J/cm @Temperature 23.0 °C |
0.0937 ft-lb/in @Temperature 73.4 °F |
ISO 180/A |
Cossa Polimeri ESTABLEND PA 1560 T8 GF ABS / Nylon 6 Blend, 30% Glass & Mineral Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.30% glass fiber and mineral fillerGood impact strength, high chemical resistance, excellent heat resistance, high dimension.. |