Mechanical Properties Metric English Comments
Izod Impact, Notched 0.267 - 4.27 J/cm
0.500 - 8.00 ft-lb/in
Average value: 0.725 J/cm Grade Count:71
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Izod Impact, Notched 1.55 - 4.27 J/cm
2.90 - 8.00 ft-lb/in
Average value: 2.82 J/cm Grade Count:8
Overview of materials for Polyphenylene Ether, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Izod Impact, Notched 3.74 - 4.27 J/cm
7.00 - 8.00 ft-lb/in
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength
BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat..
Izod Impact, Notched 3.20 - 4.27 J/cm
6.00 - 8.00 ft-lb/in
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound
BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. ..
Izod Impact, Notched 1.60 - 4.27 J/cm
3.00 - 8.00 ft-lb/in
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
Izod Impact, Notched 3.20 - 4.27 J/cm
6.00 - 8.00 ft-lb/in
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound
BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Izod Impact, Notched 1.07 - 4.27 J/cm
2.00 - 8.00 ft-lb/in
ASTM D256
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved