Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.290 - 0.850 J/cm | 0.543 - 1.59 ft-lb/in | Average value: 0.647 J/cm Grade Count:3 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.640 - 0.850 J/cm @Temperature -40.0 - -40.0 °C |
1.20 - 1.59 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.745 J/cm Grade Count:2 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.300 - 0.850 J/cm @Temperature -30.0 - 0.000 °C |
0.562 - 1.59 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.547 J/cm Grade Count:13 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.850 - 0.850 J/cm @Temperature -10.0 - 0.000 °C |
1.59 - 1.59 ft-lb/in @Temperature 14.0 - 32.0 °F |
Average value: 0.794 J/cm Grade Count:2 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.850 - 0.850 J/cm @Thickness 3.17 - 6.40 mm |
1.59 - 1.59 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 0.794 J/cm Grade Count:2 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |