Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -40.0 °C |
10.5 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Asia Pacific) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
Ineos B35-150-134 MDPE
(discontinued **) Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molde.. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 5.60 J/cm @Temperature 23.0 °C |
10.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 5.60 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
10.5 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |
|||
Izod Impact, Notched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D256A |
Braskem INSPIRE™ 117 Performance Polypropylene Polymer D 117.00 Developmental Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistanc.. |