Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
Haysite H260 Polyester Laminate Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m.. |
|||
Izod Impact, Notched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Izod Impact, Notched | 5.40 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers DIAMALOY XNY-1012U Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.40 J/cm @Thickness 3.17 mm |
10.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 2418 R UV UV Stabilized/Mold Release Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |