Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -30.0 °C |
8.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 4.30 - 5.90 J/cm | 8.06 - 11.1 ft-lb/in | Average value: 4.95 J/cm Grade Count:4 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 4.30 J/cm @Thickness 3.17 mm |
8.06 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 743 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | Plain Cast Resin; ASTM D256 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Izod Impact, Notched | 4.30 J/cm @Thickness 3.20 mm |
8.06 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 2000 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
Izod Impact, Notched | 4.30 - 5.30 J/cm @Temperature -29.0 - -29.0 °C |
8.06 - 9.93 ft-lb/in @Temperature -20.2 - -20.2 °F |
Average value: 4.63 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | edgewise; ASTM D256 |
Haysite 14200 Polyester BMC, 15% Glass Reinforced The 14200 series bulk molding compound is one of Haysite's newest molding compound families. This grade can be compression, transfer, or injection molded. Good mechanical strength and exceptional a.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | edgewise; ASTM D256 |
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | edgewise; ASTM D256 |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | edgewise; ASTM D256 |
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2) A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, .. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Haysite H-193 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset polyester sheet having good corrosion resistance to numerous acids and alkalis. This material also exhibits a high level of flame retardancy and low smoke generati.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Haysite H254 Polyester Laminate Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Haysite HCR-100 Corrosion Resistant Polyester/Glass Sheet A general purpose isophthalic polyester sheet with flame retardants and ultraviolet inhibitors. Standard color is gray. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registe.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Haysite HCR-196 Corrosion Resistant Vinyl Ester/Glass Sheet A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix. Standard color is grey. Additional data covering resistance to specific chemicals is available upon re.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | |
Spartech Royalite R84 Proprietary Polymer Weather Resistant Sheet Data provided by the manufacturer. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | Plain Cast Resin; ASTM D256 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D256 |
Engineered Plastics EPABS 19 ABS Extrusion Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 4.30 J/cm @Temperature -40.0 °C |
8.06 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ABW Polymers PC/PET Alloy Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles.. |
|||
Izod Impact, Notched | 4.30 J/cm | 8.06 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |