Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 11.6 J/cm | >= 21.7 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 11.6 J/cm | >= 21.7 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 11.6 J/cm | 21.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 11.6 J/cm | 21.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 11.6 J/cm | 21.7 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |