Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | 73°F; ASTM D256 |
Multibase Nylex™ 1404 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP340G Sheet and Thermoforming Grade Polypropylene Moplen RP340G is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340G is a random copolymer particularly suitable for.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LF1520 PC (Asia Pacific) |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP401M Injection Molding Grade Polypropylene Moplen EP401M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP401M is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
Kolon Kopa® KN153G30 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
Kolon Kopa® KN161 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Shinil Chemical SHINSTAT ABS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.75 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Zylog Hipolyene® 8025 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 340Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 640V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 640Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 54G43 43% Glass Filled Nylon 66 Enhanced strength, stiffness, and impact resistance; with 43% GF. Excellent appearance. Applications:Fans, railroad tie insulators, office furniture Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 540V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® A0501 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |