Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.43 J/cm | 2.67 ft-lb/in | 73°F; ASTM D256 |
Multibase Nylex™ 2185 R20 Natural Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL003EU PC LNP LUBRICOMP* DL003EU is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, UV Stabilized, Internally Lubricated. |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |
|||
Izod Impact, Notched | 1.43 J/cm | 2.68 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |