Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |
|||
Izod Impact, Notched | 0.950 - 7.00 J/cm | 1.78 - 13.1 ft-lb/in | Average value: 2.59 J/cm Grade Count:34 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-RG301 Flame Retardant, 30% Glass Fiber Reinforced PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech.. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Izod Impact, Notched | 0.950 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.78 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature -30.0 °C |
1.78 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL REN501 PPE+PS Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend High flow Ultem blends for thin wall application |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East) High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE002ER PC LNP STAT-KON* DE002ER is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Electrically Conductive. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance.Features: Flame Ret.. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature -30.0 °C |
1.78 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF436HR PBT PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ISO 180/A |
Styron CALIBREâ„¢ 7100-15 Polycarbonate CALIBREâ„¢ 7100-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ISO 180/A |
Styron CALIBREâ„¢ 7103-15 Polycarbonate CALIBREâ„¢ 7103-15 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBR.. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 0.000 °C |
1.78 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Asia Pacific) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm | 1.78 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1245U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1245U is a 40% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.950 J/cm @Temperature 23.0 °C |
1.78 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAESTRA G/40 40% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |