Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products M25P251-01A 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsInternal I/P componentsFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.18 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® LF-1003 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.30 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® SF-30CF/000 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
I. Stern 2335C Prime Clarified Random Copolymer Polypropylene Features:High flow characteristicsFDASee-through and contact clarityFood contact acceptableApplicationsContainersBottlesStorage boxesToysInformation provided by I. Stern & Co. Inc. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GB36 IM1 BK 36% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 36% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256A |
Total PPR 7425 Polypropylene, Injection Molding Grade Random copolymer for injection moldingClarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.Impact - FINA 7425 produced molded parts with measurably impro.. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Aclo Accutech ABS ABS833G30L Glass Reinforced |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P1-25FM-Y175 25% Glass Fiber/ Mineral Reinforced Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.30 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NL-10GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |