Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.637 J/cm | 1.19 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPET® KP133135 FR-PET Resin
(discontinued **) KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p.. |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL N109LDS POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX GP5200B PBT+ABS+GF20% Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2306FG PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.17 mm |
1.19 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.17 mm |
1.19 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HX-4300G PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.637 J/cm | 1.19 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6CV3 Flame Retardant Nylon 6, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.637 J/cm | 1.19 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NGC3 Nylon 6, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.637 J/cm | 1.19 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30BK Electric Conducting Polyformaldehyde |
|||
Izod Impact, Notched | 0.637 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.19 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G15 Nylon 6, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.637 J/cm | 1.19 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |