Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HF600N Injection Molding Grade Polypropylene Moplen HF600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HF600N is a homopolymer with improved productivity and lower energy.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP563S Fiber (Spunbond) Grade Polypropylene Moplen HP563S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP563S is a homopolymer typically used in spunb.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2056F PBT+GF5% Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 23.0 °C |
0.551 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 22.8 °C |
0.550 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5321 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Engine Cover and Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | |
Shinil Chemical SHINSTAT PP Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm |
0.551 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm |
0.551 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TK-4046H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm |
0.551 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm |
0.551 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.551 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
ExxonMobil PP1105E1 Homopolymer Product Description: High melt flow rate homopolymer. Particularly suitable for general purpose injection molding.Availability: North America Features:Controlled RheologyGeneral PurposeGood Proces.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
Cheng Yu Plastic BK1022 Electric Conducting Polypropylene, Injection |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFPP 2010 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.294 J/cm | 0.551 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30710 POM, 10% Mineral Reinforced |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | |
Abatron AboCast/AboCure 8006-11 Epoxy AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffec.. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 3.20 mm |
0.551 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS1000 Sparkle SAN Resin High Transparent SANInformation provided by Bhansali |