Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 23.0 °C |
0.500 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T40P100-01A 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Duratron® PEI U1000 LSG Polyetherimide, unfilled, extruded, Biocompatibility tested (ASTM Product Data Sheet) Duratron® U1000 (Formerly Ultem® 1000) polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it.. |
|||
Izod Impact, Notched | 0.267 - 0.801 J/cm | 0.500 - 1.50 ft-lb/in | Average value: 0.617 J/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® PP-60/TC/30 Polypropylene Homopolymer, 30% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
Ineos H12Z-02 Polypropylene Homopolymer, Antistatic and Nucleated A nucleated and antistated polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications that require superior mold release pro.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP 0096 S LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256A |
Dow 5D49 Polypropylene Homopolymer Resin OverviewConsistent processabilitySuperior spinning characteristicsComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW 5D49 Polypropylene Resin is intended for use in fiber spinning processes. It is w.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature -20.0 °C |
0.500 ft-lb/in @Temperature -4.00 °F |
molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow 6D20 Polypropylene Resin DOW 6D20 is intended for use in film and extrusion blow molding processes. It is especially suited for multilayered, barrier bottles.Information provided by DowDow Announced Sale of Global Polyprop.. |
|||
Izod Impact, Notched | 0.267 J/cm @Thickness 3.17 mm |
0.500 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9275J Amber 05 Rigid PVC, Molding, Amber 05 Georgia Gulf 9275J Amber 05 is used for injection blow molded packages in cosmetic and toiletry applications. It is a pre-colored amber compound and all ingredients are FDA approved.Information pro.. |
|||
Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256A |
Braskem FF080WP Homopolymer Polypropylene Description: Superior Color and Processing Stability, Low Odor, Excellent Clarity, Excellent Slip PropertiesApplications: Suggested Uses include Cast FilmThis resin meets the requirements for olefin.. |
|||
Izod Impact, Notched | 0.267 J/cm @Temperature 22.8 °C |
0.500 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5340 Mica Reinforced Homopolymer Information provided by Spartech |