Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | 0.125 inch bar; ASTM D256 |
Network Polymers MS 130HF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.235 - 1.07 J/cm | 0.440 - 2.00 ft-lb/in | Average value: 0.689 J/cm Grade Count:78 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Notched | 0.235 - 1.07 J/cm | 0.440 - 2.00 ft-lb/in | Average value: 0.641 J/cm Grade Count:22 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | |
Abatron AboCast 8-15/Abocure 8-15 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/11.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 70 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Izod Impact, Notched | 0.235 J/cm @Thickness 3.17 mm |
0.441 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® FT6120 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and hi.. |
|||
Izod Impact, Notched | 0.235 J/cm @Thickness 3.17 mm |
0.441 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® FT6125 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | ASTM D256 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.441 ft-lb/in | |
Zeon Chemicals Zeonex® 480 Cyclo-Olefin Polymer |
|||
Izod Impact, Notched | 0.235 J/cm | 0.441 ft-lb/in | |
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | |
Abatron AboCast 50-6/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months. |
|||
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in | |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |