Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.166 - 0.310 J/cm | 0.311 - 0.581 ft-lb/in | Average value: 0.220 J/cm Grade Count:20 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 4414 Phenolic, Granular, Injection Molded PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional .. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 5488 Phenolic, Granular, Injection Molded PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not .. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 4548 Phenolic, Granular, Injection Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Izod Impact, Notched | 0.166 J/cm | 0.311 ft-lb/in | ASTM D256 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |