Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 41 UVT LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 51 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
Plaskolite Optix® CA-71 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 41 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 87 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-81 General Purpose Acrylic Resin Extrusion Grade Pellets. Highest Molecular weight. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
NatureWorks® Ingeo™ 3001D Injection Grade PLA NatureWorks® PLA (polylactide) polymer 3001D is designed for injection molding applications. It is designed for clear applications with heat deflection temperatures lower than 130ºF (55ºC). Appli.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 42 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 51 HF General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 51 HF UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
Plaskolite West Optix® CA-71 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | 0.5 in.; ASTM D256 |
Resirene Resirene® HH-104 General Purpose Polystyrene Features:Medium FlowHigh HeatHigh Molecular WeightExternal LubricationFDA Rating: 21 CFR 177.1640Mold ReleaseApplications:InjectionPen BarrelsCassettesInformation provided by US distributor Calsak C.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPS 80-0800 Crystal Polystyrene Description: Injection Molding GradeInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.160 - 1.28 J/cm | 0.300 - 2.40 ft-lb/in | Average value: 0.506 J/cm Grade Count:27 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256-A |
Ineos Styrenics 158K High-Heat Polystyrene Crystal Resin (Global) Description: High-heat, high-molecular weight grades for a variety of applications, including medical devices and labware, cosmetics packaging, CD & DVD jewel boxes, food serviceware, and low-taste,.. |
|||
Izod Impact, Notched | 0.160 J/cm | 0.300 ft-lb/in | ASTM D256 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.300 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 280 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.160 J/cm @Thickness 6.35 mm |
0.300 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 86 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |