Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.500 - 12.0 J/cm²
2.38 - 57.1 ft-lb/in²
Average value: 2.36 J/cm² Grade Count:18
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 6.00 - 12.0 J/cm²
28.6 - 57.1 ft-lb/in²
DIN 53453
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..
Charpy Impact, Notched 0.100 - 12.0 J/cm²

@Temperature -30.0 - 0.000 °C
0.476 - 57.1 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 1.91 J/cm² Grade Count:27
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Charpy Impact, Notched 3.00 - 12.0 J/cm²

@Temperature -20.0 - 0.000 °C
14.3 - 57.1 ft-lb/in²

@Temperature -4.00 - 32.0 °F
Average value: 7.67 J/cm² Grade Count:2
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.350 - 12.0 J/cm²

@Temperature -23.0 - 0.000 °C
1.67 - 57.1 ft-lb/in²

@Temperature -9.40 - 32.0 °F
Average value: 5.20 J/cm² Grade Count:3
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 0.100 - 12.0 J/cm²

@Temperature -40.0 - 0.000 °C
0.476 - 57.1 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 0.597 J/cm² Grade Count:136
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..