Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.140 - 0.200 J/cm² | 0.666 - 0.952 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Charpy Impact, Notched | 0.150 - 0.200 J/cm² | 0.714 - 0.952 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Charpy Impact, Notched | 0.130 - 0.200 J/cm² | 0.619 - 0.952 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Charpy Impact, Notched | 0.100 - 0.200 J/cm² | 0.476 - 0.952 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact, Notched | 0.200 - 0.200 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 0.952 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.200 J/cm² Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Charpy Impact, Notched | 0.100 - 0.200 J/cm² | 0.476 - 0.952 ft-lb/in² | ISO 179 |
Vyncolit 3640 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Charpy Impact, Notched | 0.200 - 0.200 J/cm² @Temperature -20.0 - -20.0 °C |
0.952 - 0.952 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.200 J/cm² Grade Count:1 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |