Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East) LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1434T PC Copolymer (Asia Pacific) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Asia Pacific) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1494T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1494T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers extreme low temperature (-40 C) ductility in comb.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Charpy Impact, Notched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xylex X7503HP PC+POLYESTER (Europe-Africa-Middle East) Clear PC-Siloxane copolymer + Polyester alloy, USA Food ContactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | ISO Data |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Charpy Impact, Notched | 7.00 J/cm² @Temperature 23.0 °C |
33.3 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML6240 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | DAM; Partial; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |