Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.640 J/cm²

@Temperature 23.0 °C
3.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Charpy Impact, Notched 0.640 J/cm²

@Temperature -30.0 °C
3.05 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar DN101 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
ISO Data
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av..
Charpy Impact, Notched 0.640 J/cm²

@Temperature 23.0 °C
3.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG20-DN00N1 Nylon 6 20% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 0.640 J/cm²

@Temperature -30.0 °C
3.05 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar DN003 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.640 J/cm²

@Temperature 23.0 °C
3.05 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Arnite® TV4 244 S PBT-GF20 FR
20% Glass Reinforced, Flame Retardant
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® PLS FR95G15DH2 BK269 Nylon 6
15% Glass Reinforced Flame Retardant Heat Stabilized Polyamide Zytel PLSFR95G15DH2 BK269 is 15% glass reinforced flame retardant black PA using SHIELD Technology only from DuPont exceptional resista..
Charpy Impact, Notched 0.640 J/cm²

@Temperature -30.0 °C
3.05 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Appryl® 7280 Polypropylene - Polyethylene Copolymer
PP/PE copolymer colored directly or during the injection molding process. This grade with a very good impact test at low temperature, has been developed for bumpers applications for the automotive i..
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
ISO 179
BASF Ultradur S 4090 G4 BK5110 20% Glass Filled PBT
Ultradur S 4090 G4 BK5110 is a 20% glass reinforced, pigmented black PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkag..
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
ISO 179
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry)
Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830..
Charpy Impact, Notched 0.640 J/cm²
3.05 ft-lb/in²
ISO 179/1eA
Polyplastics Duracon® GH-25D Acetal Co-polymer (POM), GF 25% reinforced, High flow, High strength, High rigidity