Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.470 J/cm²

@Temperature -30.0 °C
2.24 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 105-28 Cellulose Acetate  (discontinued **)
28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.470 J/cm²
2.24 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® TD735 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 0.470 J/cm²
2.24 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® CN7740XB Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.470 J/cm²
2.24 ft-lb/in²
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..
Charpy Impact, Notched 0.470 J/cm²

@Temperature -30.0 °C
2.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Charpy Impact, Notched 0.470 J/cm²
2.24 ft-lb/in²
1eA; ISO 179
Azoty Tarnow™ TARNOFORM 300 GF3 POM
15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A...
Charpy Impact, Notched 0.470 J/cm²

@Temperature -30.0 °C
2.24 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry)
Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to ..
Charpy Impact, Notched 0.470 J/cm²

@Temperature -30.0 °C
2.24 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp..
Charpy Impact, Notched 0.470 - 1.03 J/cm²

@Temperature -30.0 - -30.0 °C
2.24 - 4.90 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.613 J/cm² Grade Count:7
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Charpy Impact, Notched 0.470 - 1.10 J/cm²
2.24 - 5.24 ft-lb/in²
Average value: 0.769 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Copyright © lookpolymers.com All Rights Reserved