Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 1.86 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179/1eA
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.390 - 0.500 J/cm²

@Temperature -30.0 - -20.0 °C
1.86 - 2.38 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.430 J/cm² Grade Count:3
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® ST25G8 Toughened Acrylic Polymer
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179/1eA
Lucite International Elvakon® 4474 High Gloss Acrylic Capstock
Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ASTM D256
Plenco 6401 Phenolic, Briquette, Injection Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 700FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
Eastman Eastapak 9921 PET
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
Arkema Group Rilsan® BMN Y BZ TL Nylon 11, Bronze Bead Filled (Conditioned)
Designation ISO 1874-PA11,MHLS,16-020,(Z+M)(B+D)(80BZ+05)Rigid grade with bronze beads (85%) and molybdenum fillers for injection molding. Available color: steel brown. Light and heat stabilized.No ..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ASTM D256
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound
ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd.
Charpy Impact, Notched 0.390 J/cm²

@Temperature -30.0 °C
1.86 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN P40 TL Nylon 12, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA12-P,EHL,22-004Flexible grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Very good chemical..
Charpy Impact, Notched 0.390 J/cm²
1.86 ft-lb/in²
ISO 179
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid B3GM35 BKQ642 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.
Charpy Impact, Notched 0.390 J/cm²

@Temperature -30.0 °C
1.86 ft-lb/in²

@Temperature -22.0 °F
ISO data
BASF Capron® 8362 HS BK-102 Impact Modified, 34% Mineral-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8362 HS BK-102 is a pigmented black, 34% mineral reinforced, impact modified, heat stabilized nylon 6 injection molding compound exhibiting a high level toughness in combination with excellen..
Charpy Impact, Notched 0.390 - 8.00 J/cm²
1.86 - 38.1 ft-lb/in²
Average value: 0.991 J/cm² Grade Count:23
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Copyright © lookpolymers.com All Rights Reserved