Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 17.0 J/cm² | >= 80.9 ft-lb/in² | ISO 179 |
Murtfeldt Material ”S”® 8000 Polyethylene Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding.. |
|||
Charpy Impact, Notched | >= 17.0 J/cm² | >= 80.9 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Charpy Impact, Notched | >= 17.0 J/cm² | >= 80.9 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® Natural Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® natural has excell.. |
|||
Charpy Impact, Notched | >= 17.0 J/cm² | >= 80.9 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Charpy Impact, Notched | >= 17.0 J/cm² | >= 80.9 ft-lb/in² | ISO 179 |
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value.. |
|||
Charpy Impact, Notched | 17.0 J/cm² | 80.9 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Charpy Impact, Notched | 17.0 J/cm² @Temperature -20.0 °C |
80.9 ft-lb/in² @Temperature -4.00 °F |
Dry; ISO 179/Af |
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |