Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | ISO 179/1eA |
Radici Radilon® AHS (dry) Nylon 66 General purposeInformation provided by Radici group. |
|||
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | |
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Charpy Impact, Notched | 0.490 J/cm² @Temperature -30.0 °C |
2.33 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 105-33 Cellulose Acetate
(discontinued **) 33% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CN5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.490 J/cm² @Temperature -30.0 °C |
2.33 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AESN Y T6L Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,MD05Grade with molybdenum filler for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Low friction coefficient. No need of l.. |
|||
Charpy Impact, Notched | 0.490 J/cm² @Temperature -30.0 °C |
2.33 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® MB 3945 Nylon 11, Rotomolding Grade (Dry) Designation ISO 1874-PA11-P,RDR,12-004Semi-rigid grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyeth.. |
|||
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | ISO 179 |
BASF Ultramid® 1310-11 NF2001 PA66 (Dry) Ultramid 1310-11 NF2001 is a controlled crystallization, fast cycling PA6/6 which provides extremely fast cycle times and improved productivity over Ultramid 1000. |
|||
Charpy Impact, Notched | 0.490 J/cm² | 2.33 ft-lb/in² | |
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Conditioned) Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro.. |
|||
Charpy Impact, Notched | 0.490 - 2.42 J/cm² @Temperature -30.0 - -30.0 °C |
2.33 - 11.5 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.17 J/cm² Grade Count:18 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |