Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.470 J/cm² @Temperature -30.0 °C |
2.24 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 105-28 Cellulose Acetate
(discontinued **) 28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.470 J/cm² | 2.24 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® TD735 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.470 J/cm² | 2.24 ft-lb/in² | ISO 179/1eA |
Polyplastics Duranex® CN7740XB Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Charpy Impact, Notched | 0.470 J/cm² | 2.24 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Charpy Impact, Notched | 0.470 J/cm² @Temperature -30.0 °C |
2.24 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.470 J/cm² | 2.24 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Charpy Impact, Notched | 0.470 J/cm² @Temperature -30.0 °C |
2.24 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® AMV TL Nylon 12, Rigid, Injection Grade (Dry) Designation ISO 1874-PA12,MHLR,16-010Rigid grade for injection molding. Available color: natural. Light and heat stabilized. Mold-release agent.High impact strength. Easy filling of the mold due to .. |
|||
Charpy Impact, Notched | 0.470 J/cm² @Temperature -30.0 °C |
2.24 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Dry) Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp.. |
|||
Charpy Impact, Notched | 0.470 - 1.03 J/cm² @Temperature -30.0 - -30.0 °C |
2.24 - 4.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.613 J/cm² Grade Count:7 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 0.470 - 1.10 J/cm² | 2.24 - 5.24 ft-lb/in² | Average value: 0.769 J/cm² Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |