Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 234 MPa @Temperature 25.0 °C |
34000 psi @Temperature 77.0 °F |
After 1500 in-in-lb/in impact, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 234 MPa @Strain 10.0 %, Temperature 23.0 °C |
33900 psi @Strain 10.0 %, Temperature 73.4 °F |
ASTM D695 Modified |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |