Polymer Property : Ball Indentation Hardness = 6960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 48.0 MPa
6960 psi
ISO 2039-1
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data)
This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to..
Ball Indentation Hardness 48.0 - 52.0 MPa
6960 - 7540 psi
ISO 2032-N132
Adamas Adalon® 403 PTFE, 15% Polyimide
Information provided by Adamas, HPM
Ball Indentation Hardness 48.0 - 52.0 MPa
6960 - 7540 psi
ISO 2032
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2
Information provided by Adamas, HPM
Ball Indentation Hardness 48.0 MPa
6960 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.