Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 48.0 MPa | 6960 psi | ISO 2039-1 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Ball Indentation Hardness | 48.0 - 52.0 MPa | 6960 - 7540 psi | ISO 2032-N132 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 48.0 - 52.0 MPa | 6960 - 7540 psi | ISO 2032 |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 48.0 MPa | 6960 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |