Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-50/4 black 9833 PA666-GF50 Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-p.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVL-6H black 9915 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Ball Indentation Hardness | 315 MPa | 45700 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-6H PA*-GF60 Product description: Grivory GV-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |