Polymer Property : Ball Indentation Hardness = 174 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 174 MPa
25200 psi
ISO 2039-1
Nilit FRIANYL B63 KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 174 MPa
25200 psi
ISO 2039-1
Nilit FRIANYL B63 GV25 Nylon 6 for injection molding, 25% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 174 MPa
25200 psi
ISO 2039-1
Nilit FRIANYL B63 W-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 174 MPa
25200 psi
ISO 2039-1
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced
Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 174 MPa
25200 psi
DIN 2039
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..