Mechanical Properties Metric English Comments
Charpy Impact 67.8 J

@Temperature -17.8 °C
50.0 ft-lb

@Temperature 0.000 °F
Universal Wire Works 70S-6 Steel Welding Wire
Universal 70S-6 is designed for welding mild steels with CO2 shielding gas. This alloy should be used where low silicon mild steel wires have not been satisfactory on slightly contaminated base meta..
Charpy Impact 67.8 J

@Treatment Temp. 1070 °C
50.0 ft-lb

@Treatment Temp. 1950 °F
austenitized; C-notch
Crucible Steel CPM® 4V® Tool Steel
CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank..
Charpy Impact 67.8 J

@Tempering Temp. 482 °C
50.0 ft-lb

@Tempering Temp. 900 °F
hardened at 1800°F then tempered; C-notch
Crucible Steel CRUCIBLE A9 Tool Steel
Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the ..
Charpy Impact 67.8 J

@Tempering Temp. 510 °C
50.0 ft-lb

@Tempering Temp. 950 °F
hardened at 1800°F then tempered; C-notch
Crucible Steel CRUCIBLE A9 Tool Steel
Crucible A9 is an air-hardening tool steel combining some of characteristics of the 5% chromium hot-work grades (such as H13) with the high attainable hardness and compressive yield strength of the ..
Charpy Impact 67.8 J

@Treatment Temp. 1040 °C
50.0 ft-lb

@Treatment Temp. 1900 °F
Solution Treated; V-notch
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel
CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm..
Charpy Impact 67.8 J

@Tempering Temp. 593 °C
50.0 ft-lb

@Tempering Temp. 1100 °F
oil quenched from 1525°F then tempered
Crucible Steel Holder Block Steel, AISI 4150 Modified
Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b..
Charpy Impact 67.8 J

@Temperature -73.3 °C
50.0 ft-lb

@Temperature -100 °F
Transverse
ATI Allegheny Ludlum AL 412™ Dual Phase 12% Cr
Low carbon, nickel containing, dual phase 12% Cr stainless steel alloy. Characteristics: superior toughness to ferritic alloys, high strength, high corrosion resistance.Information provided by Alleg..