Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 74.6 J @Treatment Temp. 760 °C, Time 7200 sec |
>= 55.0 ft-lb @Treatment Temp. 1400 °F, Time 2.00 hour |
|
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Charpy Impact | >= 74.6 J @Treatment Temp. 621 °C, Time 14400 sec |
>= 55.0 ft-lb @Treatment Temp. 1150 °F, Time 4.00 hour |
|
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Charpy Impact | 74.6 J @Temperature 300 °C |
55.0 ft-lb @Temperature 572 °F |
Longitudinal Charpy V-notch Tests from a 3" rolled plate at 293 HB |
EDRO P1FM #31 Free Machining Holder Steel EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis.. |
|||
Charpy Impact | 74.6 J @Treatment Temp. 982 °C |
55.0 ft-lb @Treatment Temp. 1800 °F |
austenitized; C-notch |
Crucible Steel CPM® 4V® Tool Steel CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank.. |
|||
Charpy Impact | 74.6 J @Treatment Temp. 593 °C |
55.0 ft-lb @Treatment Temp. 1100 °F |
hardened H1100; V-notch |
Crucible Steel CSM® 21 17Cr-4Ni Precipitation Hardening Stainless Steel CSM 21 is a precipitation hardening stainless mold steel, providing outstanding corrosion resistance and toughness, good polishability, and moderate wear resistance, combined with simple heat treatm.. |
|||
Charpy Impact | 74.6 J @Tempering Temp. 649 °C |
55.0 ft-lb @Tempering Temp. 1200 °F |
oil quenched from 1525°F then tempered |
Crucible Steel Holder Block Steel, AISI 4150 Modified Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b.. |
|||
Charpy Impact | 74.6 J @Temperature 499 °C |
55.0 ft-lb @Temperature 930 °F |
V-notch (hardness of 45 HRC) |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Charpy Impact | 74.6 J @Temperature 499 °C |
55.0 ft-lb @Temperature 930 °F |
V-notch (hardness of 45 HRC) |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |