Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 28.2 J @Thickness 3.18 mm, Temperature 23.0 °C |
20.8 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D3029 |
PolyOne Maxxam™ FR PP FR 7C11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Gardner Impact | 28.2 J | 20.8 ft-lb | ASTM D3029 |
Polymer Resources PPX/NY GP1 PPO/Nylon 66 Alloy Polyphenylene Oxide/Nylon 66 Alloy , General PurposeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Gardner Impact | 28.2 J | 20.8 ft-lb | ASTM D3029 |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Gardner Impact | 28.2 J @Temperature 23.0 °C |
20.8 ft-lb @Temperature 73.4 °F |
ASTM D5420, GB |
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA) Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa.. |
|||
Gardner Impact | 28.2 J | 20.8 ft-lb | ASTM D5420 |
Ineos Styrenics Avantra® 585K Q402 Rubber Modified Polystyrene Avantra® 585K Q402 is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical toughness. Although Avantra® 585K Q402 can be processed by any method applic.. |
|||
Gardner Impact | 28.2 J | 20.8 ft-lb | ASTM D5420 |
Ineos Styrenics Avantra® 585K Rubber Modified Polystyrene Avantra® 585K is a high-impact grade of polystyrene with extremely high surface gloss and excellent practical impact strength. Although Avantra® 585K can be processed by any method applicable.. |
|||
Gardner Impact | 28.2 J | 20.8 ft-lb | ASTM D1709 |
Multibase Multi-Flex® TPE A 5009 Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Gardner Impact | 28.2 J @Temperature -30.0 °C |
20.8 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Gardner Impact | 28.2 J @Thickness 3.17 mm, Temperature -30.0 °C |
20.8 ft-lb @Thickness 0.125 in, Temperature -22.0 °F |
Geometry GC; ASTM D5420 |
ExxonMobil PP7032E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit.. |
|||
Gardner Impact | 28.2 J @Temperature 23.0 °C |
20.8 ft-lb @Temperature 73.4 °F |
ASTM D3029 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Gardner Impact | >= 28.2 J | >= 20.8 ft-lb | ASTM D3029 |
Polymer Resources PPX/NY GP1 Modified PPO, General Purpose PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | >= 28.2 J | >= 20.8 ft-lb | ASTM D3029 |
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |