Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 18.1 J | 13.3 ft-lb | No Break at 18.1 J; ASTM D-3029 |
Multibase Multi-Flex® TPE D 4502 BLK Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo.. |
|||
Gardner Impact | 18.1 J | 13.3 ft-lb | No break; ASTM D5420-95 |
Multibase Multi-Flex® TPO D 4508 D 4508 This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase. |
|||
Gardner Impact | 18.1 J @Temperature -23.0 °C |
13.3 ft-lb @Temperature -9.40 °F |
Gardner |
Network Polymers NPP 25-2001 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 18.1 J @Temperature -30.0 °C |
13.3 ft-lb @Temperature -22.0 °F |
Gardner |
Network Polymers NPP 25-2102 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 18.1 J @Temperature -30.0 °C |
13.3 ft-lb @Temperature -22.0 °F |
Method G, geometry GC; ASTM D5420 |
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Gardner Impact | 18.1 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Gardner Impact | 18.1 J @Temperature 23.0 °C |
13.3 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Gardner Impact | 18.1 J @Thickness 3.17 mm, Temperature -28.9 °C |
13.3 ft-lb @Thickness 0.125 in, Temperature -20.0 °F |
Geometry GC; ASTM D5420 |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |
|||
Gardner Impact | 18.1 J | 13.3 ft-lb | 1.6 cm diamter tup, 0.32cm x 7.6cm x 7.6cm steel panel |
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade) 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate.. |
|||
Gardner Impact | 18.1 - 28.2 J | 13.3 - 20.8 ft-lb | Average value: 23.0 J Grade Count:4 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |