Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.77 GPa @Strain 1.80 %, Temperature 80.0 °C |
546 ksi @Strain 1.80 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Secant Modulus | 3.77 GPa @Strain 0.600 %, Temperature 0.000 °C |
546 ksi @Strain 0.600 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Secant Modulus | 3.77 GPa @Strain 0.730 %, Temperature 100 °C |
546 ksi @Strain 0.730 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |