Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 10.1 GPa @Strain 0.960 %, Temperature -20.0 °C |
1460 ksi @Strain 0.960 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Secant Modulus | 10.1 GPa @Strain 0.770 %, Temperature 0.000 °C |
1470 ksi @Strain 0.770 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Secant Modulus | 10.1 GPa @Strain 0.110 %, Temperature -40.0 °C |
1460 ksi @Strain 0.110 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 10.1 GPa @Strain 1.86 %, Temperature 23.0 °C |
1460 ksi @Strain 1.86 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Secant Modulus | 10.1 GPa @Strain 0.900 %, Temperature -40.0 °C |
1470 ksi @Strain 0.900 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 10.1 GPa @Strain 1.10 %, Temperature 23.0 °C |
1470 ksi @Strain 1.10 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 10.1 GPa @Strain 0.900 %, Temperature -40.0 °C |
1470 ksi @Strain 0.900 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |
|||
Secant Modulus | 10.1 GPa @Strain 0.231655 %, Temperature 0.000 °C |
1460 ksi @Strain 0.231655 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |
|||
Secant Modulus | 10.1 GPa @Strain 0.412778 %, Temperature 23.0 °C |
1460 ksi @Strain 0.412778 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |