Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.526 GPa @Strain 7.60 %, Temperature 40.0 °C |
76.3 ksi @Strain 7.60 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 0.526 GPa @Strain 13.0 %, Temperature 23.0 °C |
76.3 ksi @Strain 13.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |