Polymer Property : Compressive Modulus = 100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet)
Natural and Black
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet)
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet)
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet)
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption
Compressive Modulus 0.689 GPa
100 ksi
TM R050-38
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U..
Compressive Modulus 0.689 GPa
100 ksi
ASTM D695
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
Compressive Modulus 0.689 GPa
100 ksi
Stabilized, typ
Hexcel® HexWeb® HRP - 3/8 - 6.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..