Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 0.621 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.621 GPa
90.0 ksi
ASTM D695
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet)
Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM..
Compressive Modulus 0.621 GPa
90.0 ksi
Stabilized, typ
Hexcel® HexWeb® CR III 1/4-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Modulus 0.621 GPa
90.0 ksi
Stabilized, typ
Hexcel® HexWeb® HRH-10 - 1/8- 9.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Modulus 0.621 GPa
90.0 ksi
ASTM D365
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..
Compressive Modulus 0.621 GPa
90.0 ksi
Stabilized, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Copyright © lookpolymers.com All Rights Reserved