Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 47.4 MPa | 6880 psi | ASTM D695 |
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res.. |
|||
Compressive Yield Strength | 47.4 MPa | 6880 psi | ASTM D695 |
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approve.. |