Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 44.8 MPa | 6500 psi | |
Protective Coating PC-Rot Terminator® Epoxy Wood Consolidant Description: PC-Rot Terminator® is designed to strengthen decayed or rotted wood. The mixture is a low viscosity liquid that penetrates porous surfaces filling and sealing voids with an epoxy that .. |
|||
Compressive Yield Strength | 44.8 MPa @Strain 5.00 % |
6500 psi @Strain 5.00 % |
|
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |
|||
Compressive Yield Strength | 44.8 MPa | 6500 psi | TM R050-38 |
Resinlab® EP1300 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Black (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |
|||
Compressive Yield Strength | 44.8 MPa | 6500 psi | TM R050-38 |
Resinlab® EP1300 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1300 Clear (Formerly Lab Product W092602) is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It has a pot life of about one hour and .. |